Description
FILLER METAL Alloy 601 is used for gas-tungsten-arc welding of INCONEL® alloy 601. The GTAW process with FILLER METAL Alloy 601 is the only recommended joining method for applications involving temperatures over 2100° F (1150°C) or for applications at lower temperatures involving exposure to hydrogen sulfide or sulfur dioxide. The weld metal of this filler metal is comarable to the base metal in resistance to corrosion and oxidation.
C | Cr | Ni | Mn | Si | P | S | Fe | Cu | Al | Others |
.10 max | 21.0- 25.0 | 58.0- 63.0 | 1.0 max | .50 max | .03 max | .015 max | Bal. | 1.0 max | 1.0- 1.7 | .50 max |
- Specifications: AWS A5.14, SFA 5.14
- Classification: ERNiCrFe-11
TYPICAL DEPOSIT CHARACTERISTICS | ||||
---|---|---|---|---|
|