A cavity formed incidentally in metal (especially ingots) during the solidification of the last portion of liquid metal. Contraction of the metal causes this cavity or pipe. The pipe in an ingot must be removed before rolling to prevent defects such as laminations,
or cold shuts, that will reduce the strength of the product.